Synthèse de zircones mésoporeuses de haute surface

P. Trens1, W. Stichert2 and M.J. Hudson1

1  Department of Chemistry, University of Reading, P.O. Box 224, Whiteknights, Reading, Berkshire RG6 2AD, U.K.
2  Institüt fur Anorganische Chemie der Universität Marie Curie-Strasse 11, 60439 Frankfürt, Germany

Abstract
It has been shown that high surface area zirconias may be prepared by hydrolysis of ZrOCl 2 8 H 2O in the presence of surfactant (cetyltrimethylammonium bromide). The high surface area is attributed to the formation of clusters aggregated in small particles. The time of reaction between 24 and 90 hours greatly influences the specific surface area plus the extent of crystallinity of the calcined zirconias. A mechanism of synthesis leading to devised zirconium oxide is proposed.

Résumé
Il est montré que des oxydes de zirconium mésoporeux et de haute surface spécifique peuvent être préparés à partir de l'hydrolyse de ZrOCl 2 8 H 2O, en présence de tensioactif (CTAB). Les hautes aires spécifiques sont attribuées à la formation de clusters agrégés sous la forme de petites particules. Le temps de réaction est le paramètre qui paraît gouverner l'obtention des hautes aires spécifiques ainsi que la structure cristalline des matériaux calcinés. Un mécanisme de synthèse prenant en compte ces différents paramètres et conduisant à la formation d'oxydes de zirconium divisés est proposé.


Key words: caractérisation -- mésoporosité -- surface -- zircones