Activity measurement of liquid Zn-Bi alloys by EMF method
1 Dept of Materials Science and Processing, Fac of Engineering, Osaka University, 2-1 Yamadaoka, Suita, Osaka 565, Japan.
2 Max-Planck-lnstitut für Metallforschung, Institut fur Werkstoffwissenschatt, Seetrasse 92, 70174 Stuttgart, Germany.
E.M.F. of galvanic cell (-)W|Zn,ZnO|ZrO2(+Y2O3)|Zn-Bi,ZnO|W(+) was measured to determine the activity of zinc in the whole composition range at 750-950K for liquid Zn-Bi alloys. The activity of zinc in the alloys shows large positive deviations from Raoult’s law. From the activity data the concentration fluctuations at long wave length limit Scc(0) are calculated and compared with the model calculation for demixing liquid binary alloy. The miscibility gap are derived from E vs T plot.
Résumé
La f.é.m. de la pile (-)W|Zn,ZnO|ZrO2(+Y2O3)|Zn-Bi,ZnO|W(+) est measurée afin de déterminer l’activité du zinc sur tout le domaine de concentrations des alliages liquides Zn-Bi, entre 750 et 950 K. Celle-ci présente d'importants écarts positifs par rapport à la loi de Raoult. À partir des activités, on calcule, à la limite des grandes longueurs d'onde, les fluctuations de concentration Scc(0) et on les compare aux prévisions d'un modèle de démixtion des alliages binaires liquides. La lacune de miscibilité est obtenue grâce aux séries de points E vs T.
Key words: activity / e.m.f.. miscibility gap / concentration fluctuations
Mots clés : activité / f.é.m. / lacune de miscibilité / fluctuations de concentration